Modified version of process for making SiC-fiber/SiC-matrix composite material reduces damage to SiC (SCS-6) fibers and to carbon-rich coatings on fibers. Modification consists of addition of second polymer-infiltration-and-pyrolysis step to increase carbon content of porous matrix before infiltration with liquid silicon or silicon alloy.


    Access

    Access via TIB

    Check availability in my library


    Export, share and cite



    Title :

    Modified Process For Formation Of Silicon Carbide Matrix Composites


    Contributors:

    Published in:

    Publication date :

    1996-03-01



    Type of media :

    Miscellaneous


    Type of material :

    No indication


    Language :

    English


    Keywords :



    Continuous silicon carbide fiber reinforced metal matrix composites

    Mittnick, M.A. / McElman, J. | Tema Archive | 1988


    Physical properties of graphitic silicon carbide aluminium metal matrix composites

    Bell,J.A. / Stephenson,T.F. / Warner,A.E. et al. | Automotive engineering | 1997


    Physical Properties of Graphitic Silicon Carbide Aluminum Metal Matrix Composites

    Warner, A. E. M. / Bell, J. A. E. / Stephenson, T. F. et al. | SAE | 1997


    Physical Properties of Graphitic Silicon Carbide Aluminum Metal Matrix Composites

    Bell, J. A. E. / Stephenson, T. F. / Warner, A. E. M. et al. | British Library Conference Proceedings | 1997