TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi, Yield
31.01.1964
Aufsatz (Konferenz)
Englisch
TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi (276 MPa) Yield Strength
SAE Technical Papers | 1977
Titanium Tubing, Seamless Annealed, 40,000 psi (275 MPa) Yield Strength
SAE Technical Papers | 2001
TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi (276 MPa) Yield Strength
SAE Technical Papers | 1976
TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi (275 MPa) Yield Strength
SAE Technical Papers | 1994
TITANIUM TUBING, WELDED Annealed - 40,000 psi Yield
SAE Technical Papers | 1956