Temperature of the head, the waist, the bottom and angle of the bottom of same heavy rail lying on the cooling bed is tested continuously, time interval is 5min, which can provide the basis for prebending process. Additionally, the U75V 60Kg/m heavy rail straightening processes using the horizontal and edge roll compound straightening machine is discussed in this paper, and contrasts the cross-section dimension and straightness of heavy rail before and after being straightened, which is important to make certain of optimum straightening parameters.


    Zugriff

    Zugriff prüfen

    Verfügbarkeit in meiner Bibliothek prüfen

    Bestellung bei Subito €


    Exportieren, teilen und zitieren



    Titel :

    Straightness of U75V 100m Heavy Rail under Deferent Straightening Processes



    Erschienen in:

    Erscheinungsdatum :

    24.10.2011


    Format / Umfang :

    5 pages




    Medientyp :

    Aufsatz (Zeitschrift)


    Format :

    Elektronische Ressource


    Sprache :

    Englisch




    Analysis on Rail Straightness and Its Straightening Technology

    Jun, L. / Yanming, S. | British Library Conference Proceedings | 2008


    Bending Deformation of U75V Heavy Rail through Natural Cooling Process

    Song, Hua ;Tong, Shan Hu ;Jiang, Juan Juan | Trans Tech Publications | 2012


    Corrosion Behaviors of U75V, U76CrRE Heavy Rail Steel in Simulated Industrial Atmosphere

    Wang, Xiao Li ;Song, Bo ;Li, Yang Bing | Trans Tech Publications | 2013


    The Deformation Rule of the Cooled U75V Heavy Rail Caused by the Different Heat Transfer Coefficient

    Gao, Ming Xin ;Wang, Pei Long ;Jia, Hao | Trans Tech Publications | 2011